VIETNAM CUSTOMER ORDER 1 CONTAINER CERAMIC FIBER TUBER

ceramic fiber tube

1 container ceramic fiber tuber are packed for delivering to customer in Vietnam.

Ceramic fiber tube is a kind of ceramic fiber textile. The main component is aluminum silicate. It can be reinforced with alkali-free glass fiber yarn or heat-resistant steel wire. It is a refractory insulation material.
Production principle
The ceramic fiber tube mainly draws on the traditional textile production process, spinning aluminum silicate refractory fiber into yarn, and using glass fiber or heat-resistant steel wire as the reinforcing material, using special textile technology and equipment, weaving into ceramic fiber tube.
Traits
1. It is a new type of heat preservation refractory material and inorganic material. Can be used for long-term high temperature 1000°C. It contains a certain amount of binder material, and it usually burns at a lower temperature without affecting the insulation performance. It maintains good mechanical strength even after heating.
2. Light weight, high temperature resistance, good heat insulation, acid and alkali resistance, non-toxic, high tensile strength and toughness.
3. It has a higher level of electrical insulation and high temperature insulation than glass fiber casing.
4. It has good dielectric properties, chemical resistance, and superior softness and elasticity.
Features
1. Excellent heat insulation performance;
2. Low thermal conductivity, thermal shock resistance, low heat capacity
3. Excellent tensile performance;
4. Non-toxic and harmless, no harmful effects on the environment;
5. Excellent high temperature resistance strength and electrical insulation performance, long service life;
6. Excellent resistance to acid, oil, water vapor, corrosion resistance to non-ferrous metals such as zinc.
Scope of application
Used for insulation and protection machines. Including industrial motor engine and instrument heat insulation, fireproof cable covering materials, high temperature fireproof materials, and hydraulic hoses and lines, pneumatic lines, wires and high temperature resistant cables and high temperature tube packaging products, etc.
Product specifications
Casing wall thickness: 1.5-5 mm
The inner diameter is: 10-150 mm
Reinforced material: glass fiber or high temperature resistant steel wire
Weaving method: plain weaving
Working temperature: 650~1000℃
Ultimate strength: 0.03~0.05
Fiber diameter: 2~4 microns
Shrinkage (1800℉, 3H): <3%
Description
Ceramic fiber textiles contain about 15% of organic fibers. When the temperature rises for the first time, the organic fibers in the product will gradually be carbonized and blackened, and there will be smoke, and there may be flames in some places. This is a normal phenomenon and does not affect the use. As the temperature continues to rise, the product will gradually become white again, the organic fiber has been completely carbonized, and the product is entirely made of high-temperature resistant inorganic materials such as ceramic fiber.